Engineering Board Exam Reviewer · Engineering Materials · medium
The AISI–SAE designation 4340 refers to a:
- Plain carbon steel with 0.43% carbon
- Stainless steel
- Nickel–chromium–molybdenum alloy steel with 0.40% carbon
- Tool steel with 4% tungsten
Answer
C. Nickel–chromium–molybdenum alloy steel with 0.40% carbon
Solution
43xx: Ni–Cr–Mo steels.
More Engineering Materials questions
- In the AISI–SAE steel designation 1045, the last two digits indicate:
- White cast iron is hard and brittle because most of its carbon is present as:
- Ductile (nodular) cast iron contains graphite in the form of:
- Gray cast iron gets its name from the gray fracture surface caused by:
- The Hume-Rothery rules describe the conditions for:
- Which strengthening mechanism involves adding atoms of another element that dissolve in the host lattice?
- Precipitation (age) hardening is commonly used to strengthen:
- The heat treatment that restores the ductility of a cold-worked metal by forming new strain-free grains is called:
- Strengthening a metal by plastic deformation at room temperature is called:
- Prolonged heating of pearlitic steel just below the eutectoid temperature produces a very soft structure called: